Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
 
AA 5154
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  96.2 
Mg  3.5 
Cr  0.25 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.66 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 240  25  H112  more
Yield Strength (Mpa) 115 
Elongation (%) 25 
Reduction in Area (%)  
Hardness (HB500) 63  25  H112 more
Shear Strength (MPa) 150  25  H32  more
Fatigue Strength (MPa) 115  25  H112  more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 23.9  20-100  
Thermal Conductivity (W/m-K) 127  25  All 

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 54  25  All 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.