| AA 5254 | |
![]() | |
| Conditions | Tensile Properties | ||
| T (°C) | Treatment | ||
| 25 | H112 | Tensile Strength (MPa) | 240 |
| Yield Strength (MPa) | 115 | ||
| Elongation (%) | 25 | ||
| Reduction in Area (%) | |||
| 25 | H32 | Tensile Strength (MPa) | 270 |
| Yield Strength (MPa) | 205 | ||
| Elongation (%) | 15 | ||
| Reduction in Area (%) | |||
| 25 | H34 | Tensile Strength (MPa) | 290 |
| Yield Strength (MPa) | 230 | ||
| Elongation (%) | 13 | ||
| Reduction in Area (%) | |||
| 25 | H36 | Tensile Strength (MPa) | 310 |
| Yield Strength (MPa) | 250 | ||
| Elongation (%) | 12 | ||
| Reduction in Area (%) | |||
| 25 | H38 | Tensile Strength (MPa) | 330 |
| Yield Strength (MPa) | 270 | ||
| Elongation (%) | 10 | ||
| Reduction in Area (%) | |||
| 25 | O | Tensile Strength (MPa) | 240 |
| Yield Strength (MPa) | 115 | ||
| Elongation (%) | 27 | ||
| Reduction in Area (%) | |||