Metal Alloys
Alloy Home
Aluminum Alloys
General Information
Properties
Temper
Al Alloy Types
Cast Alloys
Wrought Alloys
Al Alloy List
Wrought:
   AA 1xxx
   AA 2xxx
   AA 3xxx
   AA 4xxx
   AA 5xxx
   AA 6xxx
   AA 7xxx
Cast:
   2xx.0 or x2xx.0
   3xx.0 or x3xx.0
   4xx.0 or x4xx.0
   5xx.0 or x5xx.0
   7xx.0
   8xx.0
Specific Al Alloy
General Information
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
AA 6351
Category Aluminum Alloy
Class Wrought

Composition
ElementWeight %
Al  97.8 
Si  1.0 
Mn  0.6 
Mg  0.6 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 2.6-2.8 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 70-80 25  
Tensile Strength (Mpa) 250  25  T4  more
Yield Strength (Mpa) 150 
Elongation (%) 20 
Reduction in Area (%)  
Hardness (HB500) 95  25  T6 
Shear Strength (MPa) 200  25  T6  
Fatigue Strength (MPa) 90  25  T6  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Conductivity (W/m-K) 176  25  T6 

Electric Properties
Properties Conditions 
T (°C)Treatment
Electric Resistivity (10-9W-m) 38  25  T6 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.