Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Chemical Engineering

The industry gateway for chemical engineering and plant operations.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free magazines
 
AISI 1046
ConditionsHardness
T (°C)TreatmentMethodValue
25 cold drawn (round bar (19-32 mm))  HB 187 
25 cold drawn, annealed (round bar (19-32 mm))  HB 179 
25 hot rolled (round bar (19-32 mm))  HB 170 