Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Further Details
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
 
AISI 1547
Conditions Tensile Properties 
T (°C)Treatment
25 annealed, cold drawn (round bar (19-32 mm))  Tensile Strength (MPa) 655 
Yield Strength (MPa) 585 
Elongation (%) 10 
Reduction in Area (%) 35 
25 cold drawn (round bar (19-32 mm))  Tensile Strength (MPa) 710 
Yield Strength (MPa) 605 
Elongation (%) 10 
Reduction in Area (%) 28 
25 hot rolled (round bar (19-38 mm))  Tensile Strength (MPa) 650 
Yield Strength (MPa) 360 
Elongation (%) 15 
Reduction in Area (%) 30 
Glossary
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!