Metal Alloys
Alloy Home
Steels
Carbon Steels
General Information
Properties
Classification
Low-Carbon
Medium-Carbon
High-Carbon
Other Grades
Resulfurized
High-Mn
H-Steels
Carbon Steel List
AISI 10xx
AISI 11xx
AISI 12xx
AISI 15xx
ASTM Steels
Specific Carbon Stl.
General Information
Resources
Bibliography
Reinforced Plastics

Informed and impartial coverage on the global composites industry.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free magazines
 
ASTM A569
Category Steel
Class Carbon steel

Composition
ElementWeight %
C  0.15 
Mn  0.60 
P  0.035 
S  0.04 
Cu  0.20 (min) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  