Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography
Wind Systems

Towers, turbines, gearboxes; processes for shaping and finishing component parts.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free magazines
 
AWG-32
Category Copper Alloy
Class Wire
Type Round copper wire
Designations United States: ASTM B1, ASTM B3, ASTM B258

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  