Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography
Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

more free magazines
 
AWG-35
Category Copper Alloy
Class Wire
Type Round copper wire
Designations United States: ASTM B1, ASTM B3, ASTM B258

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  