Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
UNS C10200
Conditions Tensile Properties 
T (°C)Treatment
25 (flat products, rod, wire, tube, pipe, shapes)  Tensile Strength (MPa) 221-455
Yield Strength (MPa) 69-365
Elongation (%) 55 
Reduction in Area (%)  
Note: Elongation is measured in 4 inches.
25 H55 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 275 
Yield Strength (MPa) 220 
Elongation (%) 25 
Reduction in Area (%)  
25 H80 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 380 
Yield Strength (MPa) 345 
Elongation (%)
Reduction in Area (%)  
25 OS025 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 235 
Yield Strength (MPa) 76 
Elongation (%) 45 
Reduction in Area (%)  
25 OS050 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 220 
Yield Strength (MPa) 69 
Elongation (%) 45 
Reduction in Area (%)  
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.