Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Further Details
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
UNS C23000
Conditions Tensile Properties 
T (°C)Treatment
25 (flat products, wire, tube, pipe)  Tensile Strength (MPa) 269-724
Yield Strength (MPa) 69-434
Elongation (%) 55 
Reduction in Area (%)  
Note: Elongation is measured in 3 inches.
25 H55 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 345 
Yield Strength (MPa) 275 
Elongation (%) 30 
Reduction in Area (%)  
25 H80 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 485 
Yield Strength (MPa) 400 
Elongation (%)
Reduction in Area (%)  
25 OS015 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 305 
Yield Strength (MPa) 125 
Elongation (%) 45 
Reduction in Area (%)  
25 OS050 (copper alloy tube OD=25 mm, thickness=1.65 mm)  Tensile Strength (MPa) 275 
Yield Strength (MPa) 83 
Elongation (%) 55 
Reduction in Area (%)  
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.