| UNS C44300 | |
![]() | |
| Category | Copper Alloy |
| Class | Wrought |
| Type | Inhibited admiralty copper |
| Common Names | Copper-zinc brass |
| Designations | United States: UNS C44300 |
| Composition | |
![]() | |
| Mechanical Properties | |
![]() | |
| UNS C44300 | |
![]() | |
| Category | Copper Alloy |
| Class | Wrought |
| Type | Inhibited admiralty copper |
| Common Names | Copper-zinc brass |
| Designations | United States: UNS C44300 |
| Composition | |
![]() | |
| Mechanical Properties | |
![]() | |