Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
UNS C52400
Category Copper Alloy
Class Wrought
Type Phosphor bronze, 10%D
Designations United States: UNS C52400

Composition
ElementWeight %
Cu  90.0 
Sn  10.0 
P  trace 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 455-147 25  (flat products, rod, wire) 
Yield Strength (Mpa) 193 
Elongation (%) 70 
Reduction in Area (%)  
Note: Elongation is measured in 3 inches.
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.