Metal Alloys
Alloy Home
Copper Alloys
General Information
Properties
Cu Alloy Types
Cast Alloys
Wrought Alloys
Cu Alloy List
UNS C1xxxx
UNS C2xxxx
UNS C3xxxx
UNS C4xxxx
UNS C5xxxx
UNS C6xxxx
UNS C7xxxx
UNS C8xxxx
UNS C9xxxx
Specific Cu Alloy
General Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
UNS C86500
Category Copper Alloy
Class Cast
Type Manganese bronze
Designations United States: UNS C86500, ASTM B584

Composition
ElementWeight %
Cu  58 
Sn  0.5 
Zn  39.5 
Fe  1 
Al  1 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.8-8.94 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 117 25  
Tensile Strength (Mpa) 490  25  (castings: centrifugal, investment, plaster, sand) 
Yield Strength (Mpa) 193 
Elongation (%) 30 
Reduction in Area (%)  
Hardness (HB) 130  25  (as cast) 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.