Metal Alloys
Alloy Home
Magnesium Alloys
General Information
Properties
Temper
Mg Alloys List
All
Castings
Bars and Shapes
Sheets and Plates
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Typical Physical/Mechanical Properties
Density1770-1830 kg/m3
Melting Point650 °C
Elastic Modulus44.8 GPa
Poisson's Ratio0.35
Tensile Strength152-379 MPa
Yield Strength80-280 MPa
Percent Elongation5-15%
Typical Thermal Properties
Thermal Expansion Coefficient26.1 × 10-6/K
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.