Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

more free magazines
 
AISI 4137H
Category Steel
Class Alloy steel
Type H-steel
Common Names Chromium-molybdenum steel
Designations  France: AFNOR 40 CD 4 , AFNOR 42 CD 4
Germany: DIN 1.7225
Italy: UNI 38 CrMo 4 KB , UNI 40 CrMo 4 , UNI G 4O CrMo 4
Japan: JIS SCM 4 , JIS SCM 4 H
Sweden: SS 2244
United Kingdom: B.S. 708 A 42 , B.S. 708 M 40 , B.S. 709 A40
United States: ASTM A304 , SAE J1268 , UNS H41370

Composition
ElementWeight %
C  0.34-0.41 
Mn  0.60-1.00 
Cr  0.75-1.20 
Mo  0.15-0.25 
P  0.035 
S  0.040 
Si  0.15-0.30 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  