Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
Offshore

International news and technology for marine/offshore operations around the world.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

more free magazines
 
AISI 94B17H
Category Steel
Class Alloy steel
Type H-steel
Common Names Boron steel
Designations  United States: ASTM A304 , SAE J1268 , UNS H94171

Composition
ElementWeight %
C  0.14-0.20 
Mn  0.70-1.05 
Cr  0.25-0.55 
Ni  0.25-0.65 
Mo  0.08-0.15 
P  0.035 
S  0.040 
Si  0.15-0.30 
B  0.0005-0.003 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  