Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
 
AISI Type 632
Category Steel
Class Stainless steel
Type Precipitation-hardening nonstandard
Common Names Chromium steel
Designations  Germany: DIN 1.4532
United States: AMS 5520 , AMS 5657 , AMS 5812 , AMS 5813 , ASTM A564 , ASTM A579 , ASTM A693 , ASTM A705 , SAE J467 (PH15-7-Mo) , UNS S15700

Composition
ElementWeight %
C  0.09 
Mn  1.00 
Si  1.00 
Cr  14.0-16.0 
Ni  6.5-7.75 
P  0.04 
S  0.03 
Mo  2.0-3.0 
Al  0.75-1.5 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  
Tensile Strength (Mpa) 1380  25  cold rolled (plate, sheet, strip) more
Yield Strength (Mpa) 1210 
Elongation (%)
Reduction in Area (%)  
Hardness (HRC) 41 (min)  25  cold rolled (plate, sheet, strip) more

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 9  21-93 more  
Thermal Conductivity (W/m-K) 15.1  21 more  
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.