Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

Machine Design

How-to, in-depth technical articles for machine design engineers

Chemical Engineering

The industry gateway for chemical engineering and plant operations.

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

more free magazines
 
ASTM A387 Grade 9
Category Steel
Class Alloy steel
Designations United States: UNS S50400

Composition
ElementWeight %
C  0.15 
Mn  0.30-0.60 
P  0.03 
S  0.030 
Si  1.00 
Cr  8.00-10.00 
Mo  0.90-1.10 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  