Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

NASA Tech Briefs

Innovations developed by NASA and its industry partners in a wide array of fields.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free magazines
 
ASTM A572 Grade 50
Category Steel
Class Alloy steel

Composition
ElementWeight %
C  0.23 (max) 
Mn  1.35 (max) 
P  0.04 
S  0.05 
Si  0.30 (max) 
Cu  0.20 (min) 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  