Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
Desktop Engineering

Design, simulation, test, prototyping and high performance computing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Power Transmission

Gear drives, bearings, motors, clutches, couplings, machine controls, sensors and components.

more free magazines
 
ASTM A588 Grade F
Category Steel
Class Alloy steel
Designations United States: UNS K11541

Composition
ElementWeight %
C  0.10-0.20 
Mn  0.50-1.00 
P  0.04 
S  0.05 
Si  0.30 (max) 
Cr  0.30 (max) 
Ni  0.40-1.10 
Mo  0.10-0.20 
V  0.01-0.10 
Cu  0.30-l.00 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  