Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
General Information
Resources
Bibliography
World Pumps

Major news, innovation and real-life applications for pumps and ancillary equipment.

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

Hydraulics & Pneumatics

For design and manufacturing engineers involved in buying or specifying fluid power components and systems.

Laser Solutions

Cost-effective laser solutions for many manufacturing problems.

more free magazines
 
ASTM A633 Grade C
Category Steel
Class Alloy steel
Designations United States: UNS K12000

Composition
ElementWeight %
C  0.20 (max) 
Mn  1.15-1.50 
P  0.04 
S  0.05 
Si  0.15-0.50 
Nb  0.01-0.05 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 7.7-8.03 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  