TM">
Metal Alloys
Alloy Home
Steels
Stainless Steels
General Information
Properties
Stainless Stl. Grades
Austenitic
Martensitic
Ferritic
Precipitation Hardening
Stainless Steel List
AISI Type 2xx
AISI Type 3xx
AISI Type 4xx
AISI Type 5xx
AISI Type 6xx
* For other AISI or Non-AISI, please use the search function above or check Grades.
Specific Stainless Stl
TM">General Information
Further Details
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?

more free publications
 
Custom455TM
Conditions Tensile Properties 
T (°C)Treatment
25 H900 (bar)  Tensile Strength (MPa) 1620 
Yield Strength (MPa) 1520 
Elongation (%)
Reduction in Area (%) 30 
25 H950 (plate, sheet, strip)  Tensile Strength (MPa) 1530 
Yield Strength (MPa) 1410 
Elongation (%)
Reduction in Area (%)  
25 H950 (bar)  Tensile Strength (MPa) 1520 
Yield Strength (MPa) 1410 
Elongation (%) 10 
Reduction in Area (%) 40 
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Salary Expectation

8 things to know about the interview question "What's your salary expectation"?