Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Further Details
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

more free publications
 
Ti-8Al-1Mo-1V
Conditions Tensile Properties 
T (°C)Treatment
25 duplex annealed   Tensile Strength (MPa) 1000 
Yield Strength (MPa) 951 
Elongation (%) 15 
Reduction in Area (%) 28 
315 duplex annealed   Tensile Strength (MPa) 793 
Yield Strength (MPa) 621 
Elongation (%) 20 
Reduction in Area (%) 38 
425 duplex annealed   Tensile Strength (MPa) 738 
Yield Strength (MPa) 565 
Elongation (%) 20 
Reduction in Area (%) 44 
540 duplex annealed   Tensile Strength (MPa) 621 
Yield Strength (MPa) 517 
Elongation (%) 25 
Reduction in Area (%) 55 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.