Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Resources
Bibliography
Offshore

International news and technology for marine/offshore operations around the world.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

Design-2-Part

How OEM's can make their parts better, faster, and more efficient.

Chemical Engineering

The industry gateway for chemical engineering and plant operations.

more free magazines
 
Ti-6Al-4V
Category Titanium Alloy
Class Wrought
Type Alpha-beta alloy
Designations United States: ASTM B265 Grade5, ASTM B348 Grade5, ASTM B381 Grade5, MIL-T-9046, MIL-T-9047, AMS 4928, AMS 4911, AMS 4906, AMS 4965

Composition
ElementWeight %
Al  6 
V  4 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 4.43 25  
Poisson's Ratio 0.34 25  
Elastic Modulus (GPa) 113.8 25  
Tensile Strength (Mpa) 993  25  annealed  more
Yield Strength (Mpa) 924 
Elongation (%) 14 
Reduction in Area (%) 30 
Hardness (HRC) 36  25  annealed more
Impact Strength (J)
(Charpy)
19  25  annealed  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 8.6  20-100 more  