Ti-6Al-4V
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
20-100   8.6 
20-205   9 
20-315   9.2 
20-425   9.4 
20-540   9.5 
20-650   9.7 