Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
 
Ti-13V-11Cr-3Al
Category Titanium Alloy
Class Wrought
Type Beta alloy
Designations United States: MIL-T-9046, AMS 4917

Composition
ElementWeight %
V  13 
Cr  11 
Al  3 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 4.84 25  
Poisson's Ratio 0.3 25  
Elastic Modulus (GPa) 101.4 25  
Tensile Strength (Mpa) 1276  25  solution+age  
Yield Strength (Mpa) 1207 
Elongation (%) 8 
Reduction in Area (%)  
Hardness (HRC) 40  25  solution+age 
Impact Strength (J)
(Charpy)
11  25  solution+age  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 9.4  20-100 more  
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.