Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Further Details
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

more free publications
 
99.2 Ti
Conditions Tensile Properties 
T (°C)Treatment
25 annealed   Tensile Strength (MPa) 434 
Yield Strength (MPa) 345 
Elongation (%) 28 
Reduction in Area (%) 50 
315 annealed   Tensile Strength (MPa) 193 
Yield Strength (MPa) 117 
Elongation (%) 35 
Reduction in Area (%) 75 
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.