Metal Alloys
Alloy Home
Titanium Alloys
General Information
Properties
Ti Alloys List
All
Commercially Pure
Alpha Alloys
Near Alpha Alloys
Alpha-Beta Alloys
Beta Alloys
Specific Ti Alloy
General Information
Resources
Bibliography
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
Ti-5Al-2.5Sn
Category Titanium Alloy
Class Wrought
Type Alpha alloy
Designations United States: ASTM B265 Grade6, ASTM B348 Grade6, ASTM B381 Grade6, MIL-T-9046, MIL-T-9047, AMS 4926, AMS 4910, AMS 4966, AMS 4953

Composition
ElementWeight %
Al  5 
Sn  2.5 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 4.48 25  
Poisson's Ratio 0.33 25  
Elastic Modulus (GPa) 110.3 25  
Tensile Strength (Mpa) 565  315 more annealed  
Yield Strength (Mpa) 448 
Elongation (%) 18 
Reduction in Area (%) 45 
Hardness (HRC) 36  25  annealed 
Impact Strength (J)
(Charpy)
26  25  annealed  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 9.4  20-100 more  
Glossary
Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.