Metal Alloys
Alloy Home
Steels
Tool Steels
General Information
Properties
Tool Steel Types
High-Speed
Hot-Work
Cold-Work
Shock-Resistant
Mold
Special-Purpose
Water-Hardening
Tool Steel List
AISI Ax
AISI Dx
AISI Hx
AISI Lx
AISI Mx
AISI Ox
AISI Px
AISI Sx
AISI Tx
AISI Wx
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
Found 17 records
Steel
Name Class Alloy Type
AISI A10  Tool steel  Air-hardening medium-alloy cold work steel 
AISI A2  Tool steel  Air-hardening medium-alloy cold work steel 
AISI A3  Tool steel  Air-hardening medium-alloy cold work steel 
AISI A4  Tool steel  Air-hardening medium-alloy cold work steel 
AISI A6  Tool steel  Air-hardening medium-alloy cold work steel 
AISI A7  Tool steel  Air-hardening medium-alloy cold work steel 
AISI A8  Tool steel  Air-hardening medium-alloy cold work steel 
AISI A9  Tool steel  Air-hardening medium-alloy cold work steel 
AISI D2  Tool steel  High-carbon, high-chromium cold work steel 
AISI D3  Tool steel  High-carbon, high-chromium cold work steel 
AISI D4  Tool steel  High-carbon, high-chromium cold work steel 
AISI D5  Tool steel  High-carbon, high-chromium cold work steel 
AISI D7  Tool steel  High-carbon, high-chromium cold work steel 
AISI O1  Tool steel  Oil-hardening cold work steel 
AISI O2  Tool steel  Oil-hardening cold work steel 
AISI O6  Tool steel  Oil-hardening cold work steel 
AISI O7  Tool steel  Oil-hardening cold work steel 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.