Metal Alloys
Alloy Home
Steels
Tool Steels
General Information
Properties
Tool Steel Types
High-Speed
Hot-Work
Cold-Work
Shock-Resistant
Mold
Special-Purpose
Water-Hardening
Tool Steel List
AISI Ax
AISI Dx
AISI Hx
AISI Lx
AISI Mx
AISI Ox
AISI Px
AISI Sx
AISI Tx
AISI Wx
Specific Tool Steel
General Information
Resources
Bibliography
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
 
AISI T5
Category Steel
Class Tool steel
Type Tungsten high speed steel
Designations  Germany: DIN 1.3265
Italy: UNI KU
Japan: JIS SKH 4A
United Kingdom: B.S. BT 5
United States: ASTM A600 , FED QQ-T-590 , SAE J437 , SAE J438 , UNS T12005

Composition
ElementWeight %
C  0.75-0.85 
Mn  0.20-0.40 
Si  0.20-0.40 
Cr  3.75-5.00 
Ni  0.3 
Mo  0.50-1.25 
W  17.50-19.00 
V  1.80-2.40 
Co  7.00-9.50 
Cu  0.25 
P  0.03 
S  0.03 

Mechanical Properties
Properties Conditions 
T (°C)Treatment
Density (×1000 kg/m3) 8.75 25  
Poisson's Ratio 0.27-0.30 25  
Elastic Modulus (GPa) 190-210 25  

Thermal Properties
Properties Conditions 
T (°C)Treatment
Thermal Expansion (10-6/ºC) 11.2  20-100 more  
Glossary
Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.