Metal Alloys
Alloy Home
Steels
Tool Steels
General Information
Properties
Tool Steel Types
High-Speed
Hot-Work
Cold-Work
Shock-Resistant
Mold
Special-Purpose
Water-Hardening
Tool Steel List
AISI Ax
AISI Dx
AISI Hx
AISI Lx
AISI Mx
AISI Ox
AISI Px
AISI Sx
AISI Tx
AISI Wx
Specific Tool Steel
General Information
Further Details
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

more free publications
 
AISI W1
ConditionsThermal Expansion Coeff. (10-6/ºC)
T (°C)Treatment
20-100   10.4 
20-200   11 
20-425   13.1 
20-500   13.8 
20-600   14.2 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.