Metal Alloys
Alloy Home
Steels
Tool Steels
General Information
Properties
Tool Steel Types
High-Speed
Hot-Work
Cold-Work
Shock-Resistant
Mold
Special-Purpose
Water-Hardening
Tool Steel List
AISI Ax
AISI Dx
AISI Hx
AISI Lx
AISI Mx
AISI Ox
AISI Px
AISI Sx
AISI Tx
AISI Wx
Specific Tool Steel
General Information
Further Details
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

more free publications
 
AISI W1
ConditionsThermal Conductivity (W/m-K)
T (°C)Treatment
100   48.3 
260   41.5 
400   38.1 
540   34.6 
675   29.4 
815   24.2 
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.