Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
Carbon
6
C
12.011
Atomic Number 6
Atomic Weight 12.011
Electron Config. 2-2-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Modulus of Elasticity 6.895 GPa Solid  0   

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.375 W-m 273.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 4765.15 K   Triple point 
Boiling Temperature
*Sublimation temperature.
3915.15 K   101325 
Critical Temperature 7200 K    
 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.