Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
Chromium
24
Cr
51.9961
Atomic Number 24
Atomic Weight 51.9961
Electron Config. 2-2-6-2-6-5-1
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 7150 kg/m3 Solid  298.15 
Modulus of Elasticity 248.211 GPa Solid  0   
Poisson Ratio 0.31 Solid     
Thermal Expansion Coefficient 4.900 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.290 W-m 273.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 2180.15 K   101325 
Boiling Temperature 2944.15 K   101325 
Critical Temperature 5500 K    
Fusion Enthalpy 404 J/g 101325 
Heat Capacity 449 J/kg-K 298.149993896 more... 100000 
Thermal Conductivity 93.7 W/m-K 300 more... 101325 
 
Glossary
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.