Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
Cesium
55
Cs
132.905
Atomic Number 55
Atomic Weight 132.905
Electron Config. 2-2-6-2-6-10-2-6-10-0-2-6-0-0-1
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 1930 kg/m3 Solid  298.15  0 
Thermal Expansion Coefficient 9.700 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 2.000 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 301.59 K   101325 
Boiling Temperature 944.15 K   101325 
Critical Temperature 2015 K    
Fusion Enthalpy 15.8 J/g 0  101325 
Heat Capacity 242 J/kg-K 298.149993896 100000 
Thermal Conductivity 35.9 W/m-K 300 101325 
 
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.