Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Germanium
32
Ge
72.61
Atomic Number 32
Atomic Weight 72.61
Electron Config. 2-2-6-2-6-10-2-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 5320 kg/m3 Solid  0  0 
Thermal Expansion Coefficient 5.750 /K Solid  293.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 0.4600 W-m 295.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1211.4 K   101325 
Boiling Temperature 3106.15 K   101325 
Critical Temperature 8900 K    
Fusion Enthalpy 508.9 J/g 0  101325 
Vaporization Enthalpy 4599.92 J/g 0  101325 
Heat Capacity 320 J/kg-K 298.149993896 more... 100000 
Thermal Conductivity 59.9 W/m-K 300 more... 101325 
 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.