Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

more free publications
Lithium
3
Li
6.941
Atomic Number 3
Atomic Weight 6.941
Electron Config. 2-1
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 534 kg/m3 Solid  298.15  0 
Thermal Expansion Coefficient 4.600 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 8.550 W-m 273.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 453.65 K   101325 
Boiling Temperature 1615.15 K   101325 
Critical Temperature 3700 K    
Fusion Enthalpy 432 J/g 0  101325 
Heat Capacity 3582 J/kg-K 298.149993896 more... 100000 
Thermal Conductivity 84.7 W/m-K 300 101325 
 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.