Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Quality Magazine

Techniques to improve quality on the shop floor and in manufacturing planning.

Autonomous Vehicle Engineering

The No. 1 media source for those developing the next generation mobility solutions.

more free magazines
Neodymium
60
Nd
144.24
Atomic Number 60
Atomic Weight 144.24
Electron Config. 2-2-6-2-6-10-2-6-10-4-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 7010 kg/m3 Solid  298.15 
Poisson Ratio 0.28 Solid     
Thermal Expansion Coefficient 9.600 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 6.400 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1289.15 K   101325 
Boiling Temperature 3339.15 K   101325 
Critical Temperature 7900 K    
Fusion Enthalpy 49.5 J/g 101325 
Heat Capacity 190 J/kg-K 298.149993896 100000 
Thermal Conductivity 16.5 W/m-K 300 101325 
 