Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
Neptunium
93
Np
[237]
Atomic Number 93
Atomic Weight [237]
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-10-4-2-6-1-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 20200 kg/m3 Solid  298.15  0 

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 917.15 K   101325 
Boiling Temperature 4160 K   101325 
Critical Temperature 12000 K    
Thermal Conductivity 6.3 W/m-K 300 101325 
 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.