Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Phosphorus
15
P
30.9738
Atomic Number 15
Atomic Weight 30.9738
Electron Config. 2-2-6-2-3
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 1830 kg/m3 Solid  0 

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.000 W-m 284.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 317.3 K   101325 
Boiling Temperature 553.65 K   101325 
Critical Temperature 994.15 K    
Vaporization Enthalpy 458.45 J/g 298.15  101325 
Vaporization Enthalpy 400.34 J/g 101325 
 
Glossary
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.