Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Radon
86
Rn
[222]
Atomic Number 86
Atomic Weight [222]
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-10-0-2-6
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 9.96 kg/m3 Gas  293.15  101325 

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 202.15 K   101325 
Boiling Temperature 211.45 K   101325 
Critical Temperature 377.15 K    
Fusion Enthalpy 12.3 J/g 101325 
Heat Capacity 94 J/kg-K 298.149993896 100000 
 
Glossary
Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.