Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
Antimony
51
Sb
121.76
Atomic Number 51
Atomic Weight 121.76
Electron Config. 2-2-6-2-6-10-2-6-10-0-2-3
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 6680 kg/m3 Solid  298.15 
Modulus of Elasticity 75.842 GPa Solid  0   
Thermal Expansion Coefficient 1.100 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 3.900 W-m 273.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 903.78 K   101325 
Boiling Temperature 1860.15 K   101325 
Critical Temperature 5700 K    
Fusion Enthalpy 163.2 J/g 101325 
Heat Capacity 207 J/kg-K 298.149993896 100000 
Thermal Conductivity 24.3 W/m-K 300 101325 
 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!