Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Terbium
65
Tb
158.925
Atomic Number 65
Atomic Weight 158.925
Electron Config. 2-2-6-2-6-10-2-6-10-9-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 8230 kg/m3 Solid  298.15 
Poisson Ratio 0.26 Solid     
Thermal Expansion Coefficient 1.030 /K Solid  298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1632.15 K   101325 
Boiling Temperature 3494.15 K   101325 
Critical Temperature 8470 K    
Fusion Enthalpy 63.9 J/g 101325 
Heat Capacity 182 J/kg-K 298.149993896 100000 
Thermal Conductivity 11.1 W/m-K 300 101325 
 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Essentials of Manufacturing

Information, coverage of important developments and expert commentary in manufacturing.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.