Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

more free publications
Titanium
22
Ti
47.867
Atomic Number 22
Atomic Weight 47.867
Electron Config. 2-2-6-2-6-2-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 4510 kg/m3 Solid  298.15 
Modulus of Elasticity 117.211 GPa Solid  0   
Poisson Ratio 0.32 Solid     
Thermal Expansion Coefficient 8.600 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 4.200 W-m 293.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1941.15 K   101325 
Boiling Temperature 3560.15 K   101325 
Critical Temperature 5850 K    
Fusion Enthalpy 295 J/g 101325 
Heat Capacity 523 J/kg-K 298.149993896 more... 100000 
Thermal Conductivity 21.9 W/m-K 300 more... 101325 
 
Glossary
Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.