Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

more free publications
Thallium
81
Tl
204.383
Atomic Number 81
Atomic Weight 204.383
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-10-0-2-1
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 11800 kg/m3 Solid  298.15  0 
Poisson Ratio 0.45 Solid     
Thermal Expansion Coefficient 2.990 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 1.800 W-m 273.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 577.15 K   101325 
Boiling Temperature 1746.15 K   101325 
Critical Temperature 4550 K    
Fusion Enthalpy 20.3 J/g 0  101325 
Heat Capacity 129 J/kg-K 298.149993896 100000 
Thermal Conductivity 46.1 W/m-K 300 101325 
 
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.