Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
Tungsten
74
W
183.84
Atomic Number 74
Atomic Weight 183.84
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-4-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 19300 kg/m3 Solid  298.15  0 
Modulus of Elasticity 344.738 GPa Solid  0   
Poisson Ratio 0.28 Solid     
Thermal Expansion Coefficient 4.500 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 5.650 W-m 300.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 3695.15 K   101325 
Boiling Temperature 5828.15 K   101325 
Critical Temperature 15500 K    
Fusion Enthalpy 284.5 J/g 0  101325 
Heat Capacity 132 J/kg-K 298.149993896 more... 100000 
Thermal Conductivity 174 W/m-K 300 more... 101325 
 
Glossary
CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Injection Molding Design Guide

Guide for high quality and cost-effective plastic injection molding.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.