Materials Home
Pure Elements
Periodic Table
Element List
  by Name
  by Symbol
  by Atomic Number
  by Atomic Weight
Element Information
Resources
Bibliography
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

more free publications
Ytterbium
70
Yb
173.04
Atomic Number 70
Atomic Weight 173.04
Electron Config. 2-2-6-2-6-10-2-6-10-14-2-6-0-0-2
Electron configuration order: 1s-2s-2p-3s-3p-3d-4s-4p-4d-4f-5s-5p-5d-5f-6s-6p-6d-7s

Mechanical Properties Conditions
Phase Temp. (K) Pressure (Pa)
Density 6900 kg/m3 Solid  298.15 
Poisson Ratio 0.21 Solid     
Thermal Expansion Coefficient 2.630 /K Solid  298.15  

Electrical Properties Conditions
Temp. (K) Note
Electrical Resistivity 2.900 W-m 298.15  

Thermal Properties Conditions
Temp. (K) Pressure (Pa)
Melting Temperature 1097.15 K   101325 
Boiling Temperature 1467.15 K   101325 
Critical Temperature 4080 K    
Fusion Enthalpy 44.3 J/g 101325 
Heat Capacity 155 J/kg-K 298.149993896 100000 
Thermal Conductivity 38.5 W/m-K 300 101325 
 
Glossary
3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.

Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.