Materials Home
Common Materials
Solids
Liquids
Gases
Specific Materials
Elements
Metal Alloys
Polymers
Piezo Materials
Solders
Steam Tables
Saturated Steam
Wet Steam
General
Resources
Bibliography
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

more free publications
Saturated Steam Table
The Temperature and the Pressure of the saturated steam are mutually dependent. When one of them is given, the other is determined. Please enter either the temperature or the pressure, and click on the "Go" button to proceed. For water or steam other than saturated steam, please use the general steam table. If you know the dryness of the steam, you may want to use the wet steam table instead.
Temperature (T)
OR
Absolute Pressure (P)
Properties of the saturated steam are listed below in both metric and standard units. To convert any value to other units, click on the number itself.
Property Metric Standard
State Saturated Steam
Use the general steam table for non-saturated steam
Temperature (T) 100.00 C 212.00 F
Pressure (P) 1.0142 bar 14.710 psi
Density Saturated Liquid (rhof) 958.35 kg/m3 59.828 lb/ft3
Saturated Vapor (rhog) 0.59816 0.037342
Specific Volume Saturated Liquid (vf) 0.0010435 m3/kg 0.016715 ft3/lb
Saturated Vapor (vg) 1.6718 26.780
Enthalpy Saturated Liquid (hf) 419.17 kJ/kg 180.21 Btu/lb
Evaporated (hfg) 2256.4 970.1
Saturated Vapor (hg) 2675.6 1150.3
Entropy Saturated Liquid (sf) 1.3072 kJ/kg-K
(mayer)
0.31222 Btu/lb-R
Evaporated (sfg) 0 0
Saturated Vapor (sg) 7.3541 1.7565
Glossary
Selecting the Right 3D Printer

Discover how to choose the right 3D printer for your needs and the key performance attributes to consider.

Mechanical Engineers Outlook

Guide for those interested in becoming a mechanical engineer. Includes qualifications, pay, and job duties.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!