Glossary » Design » Oring » Chemical » Corn Oil

Common O-Ring materials that are SUITABLE for dynamic and static seal in the environment containing Corn Oil include

  • Buna-N (Nitrile): Buna-N, also known as Nitrile rubber, is a synthetic rubber copolymer of acrylonitrile (ACN) and butadiene.
  • Chemraz: Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE.
  • Epichlorohydrin: Epichlorohydrin (ECO) has properties similar to nitrile rubber but with better heat and oil resistance as well as better low temperature flexibility.
  • Fluorocarbon: Fluorocarbon elastomer (FKM) material is also known by its tradename VITON or Fluorel.
  • Fluorosilicone: Fluorosilicone combines excellent low-temperature performance of silicone with improved chemical resistance.
  • Kalrez: Kalrez is the tradename for a perfluoroelastomeric material.
  • Hydrogenated Nitrile: Hydrogenated Nitrile Butadiene Rubber (HNBR) is also known as Highly Saturated Nitrile (HSN).
  • Polyacrylate: Polyacrylate (ACM) is a class of copolymer of ethyl and acrylates.
  • Millable Polyurethane: Millable Polyurethane rubber is made from both polyester and polyether polyols.
  • Silicone: Silicone is a semi-organic elastomer with outstanding resistance to extremes of temperature.
  • Virgin Teflon: Because Teflon is a hard plastic rather than a stretchy elastomer, it is uncommon to see an o-ring that is made entirely of Teflon.
  • Vamac: Vamac is the tradename of a class of Ethylene Acrylic elastomer (AEM).

The O-Ring materials below are USUALLY SUITABLE for static seal in the environment containing Corn Oil.

  • Butyl: Butyl (IIR) is a synthetic rubber, a copolymer of isobutylene and isoprene.
  • Hypalon: Hypalon is the traenme of a clasof Chlorosulfonated Polyethylene (CSM).

O-Ring materials that are NOT SUITABLE for using in the environment containing Corn Oil include

  • Natural Rubber: Natural rubber is a product coagulated from the latex of the rubber tree, hevea brasiliensis.
  • Polysulfide: Polysulfide was one of the first commercial synthetic elastomers.
  • Styrene Butadiene: Styrene-Butadiene rubber (SBR) has properties similar to those of natural rubber.
Additional Information

There is not enough data to determine whether the following common O-Ring materials are suitable for using in the environment containing Corn Oil or not.

  • Aflas: Aflas is the tradename for a unique fluoroelastomer based upon an alternating copolymer of tetrafluoroethylene and propylene ("TFE/P").
  • Ethylene-Propylene: Ethylene-propylene (EP) is a copolymer of ethylene and propylene.
  • Neoprene: Neoprene is a homopolymer of chlorobutadiene (CR).
  • Cast Polyurethane: Cast Polyurethane exhibits outstanding tensile strength and abrasion resistance in comparison with other elastomers.
Related Pages
STEM Career Outlook

Wages, employment opportunities, and growth projections for STEM jobs.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.