Glossary » Design » Oring » Chemical » Diphenyl

Common O-Ring materials that are SUITABLE for dynamic and static seal in the environment containing Diphenyl include

  • Aflas: Aflas is the tradename for a unique fluoroelastomer based upon an alternating copolymer of tetrafluoroethylene and propylene ("TFE/P").
  • Chemraz: Chemraz combines the resilience and sealing force of an elastomer with chemical resistance approaching that of PTFE.
  • Fluorocarbon: Fluorocarbon elastomer (FKM) material is also known by its tradename VITON or Fluorel.
  • Kalrez: Kalrez is the tradename for a perfluoroelastomeric material.
  • Virgin Teflon: Because Teflon is a hard plastic rather than a stretchy elastomer, it is uncommon to see an o-ring that is made entirely of Teflon.

The O-Ring materials below are USUALLY SUITABLE for static seal in the environment containing Diphenyl.

  • Fluorosilicone: Fluorosilicone combines excellent low-temperature performance of silicone with improved chemical resistance.
  • Polysulfide: Polysulfide was one of the first commercial synthetic elastomers.

O-Ring materials that are NOT SUITABLE for using in the environment containing Diphenyl include

  • Buna-N (Nitrile): Buna-N, also known as Nitrile rubber, is a synthetic rubber copolymer of acrylonitrile (ACN) and butadiene.
  • Butyl: Butyl (IIR) is a synthetic rubber, a copolymer of isobutylene and isoprene.
  • Ethylene-Propylene: Ethylene-propylene (EP) is a copolymer of ethylene and propylene.
  • Hypalon: Hypalon is the traenme of a clasof Chlorosulfonated Polyethylene (CSM).
  • Natural Rubber: Natural rubber is a product coagulated from the latex of the rubber tree, hevea brasiliensis.
  • Neoprene: Neoprene is a homopolymer of chlorobutadiene (CR).
  • Hydrogenated Nitrile: Hydrogenated Nitrile Butadiene Rubber (HNBR) is also known as Highly Saturated Nitrile (HSN).
  • Polyacrylate: Polyacrylate (ACM) is a class of copolymer of ethyl and acrylates.
  • Millable Polyurethane: Millable Polyurethane rubber is made from both polyester and polyether polyols.
  • Silicone: Silicone is a semi-organic elastomer with outstanding resistance to extremes of temperature.
  • Styrene Butadiene: Styrene-Butadiene rubber (SBR) has properties similar to those of natural rubber.
Additional Information

There is not enough data to determine whether the following common O-Ring materials are suitable for using in the environment containing Diphenyl or not.

  • Epichlorohydrin: Epichlorohydrin (ECO) has properties similar to nitrile rubber but with better heat and oil resistance as well as better low temperature flexibility.
  • Cast Polyurethane: Cast Polyurethane exhibits outstanding tensile strength and abrasion resistance in comparison with other elastomers.
  • Vamac: Vamac is the tradename of a class of Ethylene Acrylic elastomer (AEM).
Related Pages
Metal 3D Printing Design Guide

Direct Metal Laser Sintering (DMLS) 3D printing for parts with reduced cost and little waste.

CNC Machining Design Guide

Optimize your designs, reduce machining time, and lower your costs.

Negotiate Your Salary

Learn the best principles to negotiate the salary you deserve!

3D Scanners

A white paper to assist in the evaluation of 3D scanning hardware solutions.